庆阳外墙*离心玻璃棉板导热系数

高温玻璃棉施工建议 

在设备表面提前焊上销钉,再用铁丝把高温玻璃棉捆绑在设备表面,当所需保温的设备温度超过250℃时,采用双层保温方式,内外两层玻璃棉的接缝应错开,以免产生热桥造成热量损失。当所需保温的设备温度超过400℃时,建议内层用一定厚度的硅酸铝,外层用耐高温玻璃棉,两层之间的接缝也应错开。zui后在外面包上外裹层,既可保护玻璃棉,又达到美观的要求。报价: 

 

First, weld pins to the surface of the equipment in advance and then tie the refractory glass wool over the surface of the equipment. If temperature of the equipment is above 250℃, it is recommendable to adopt double-layer heat preservation method. Make sure that the seams of the outer and inner layers of glass wool are staggered to avoid heat loss due to the heat bridge formed. If temperature of the equipment exceeds 400℃, it is recommendable to use aluminum silicate for the inner layer and refractory glass wool for the outer layer, also staggering their seams. Finally, wrap the outer cover layer which serves both as protection to the glass wool and decoration. 

超细玻璃棉主要物理性能指标 

项目 

单位 

指标 

标准 

密度 

Kg/m3 

10-100 

GB/T 5480.3-1985 

纤维平均直径 

μ m 

5.5 

GB/T 5480.4-1985 

含水率 

≤1 

GB/T 3007-1982 

燃烧性能级别 

  

不燃* 

GB 8624-1997 

热荷重收缩温度 

℃ 

≥250 

GB/T 11835-1988 

导热系数 

w/m·k 

0.038-0.06 

GB/T 10294-1988 

憎水率 

≥98.2 

GB/T 10299-1988 

吸湿性 

≤5 

GB/T 16401-1986 

吸声系数 

  

1.03产品混声定法
24kg/m3 2000HZ 

GBJ47-83 

渣球含量 

≤0.3 

  

 

玻璃棉产品规格 

产品 

Product 

长度(mm) 

Length 

宽度(mm) 

Width 

厚度(mm) 

Thickness 

密度(Kg/m3) 

Density 

板材 

Boards 

1200-2200 

600-1200 

20-100 

24-96 

卷毡 

Blanket 

rolls  

11000,20000 

1200 

25-150 

12,16,20,24,32,40,48